2018
DOI: 10.19026/ajfst.14.5887
|View full text |Cite
|
Sign up to set email alerts
|

Electrochemical Study of Cassava Starch Conductive Biopolymers Synthesized at Different pH

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…The solutions were heated to 70 • C using constant stirring for 15 min. After the heating process, the solutions were poured into Teflon Petri dishes, which were placed in an oven for 48 h at a temperature of 70 • C. The films formed were left undisturbed for 24 h at room temperature [30,31]. Each of the films was prepared in triplicate to report the average value of the measurements carried out.…”
Section: Biopolymer Composite Film Synthesis Processmentioning
confidence: 99%
“…The solutions were heated to 70 • C using constant stirring for 15 min. After the heating process, the solutions were poured into Teflon Petri dishes, which were placed in an oven for 48 h at a temperature of 70 • C. The films formed were left undisturbed for 24 h at room temperature [30,31]. Each of the films was prepared in triplicate to report the average value of the measurements carried out.…”
Section: Biopolymer Composite Film Synthesis Processmentioning
confidence: 99%