2021
DOI: 10.1016/j.ijrmhm.2021.105689
|View full text |Cite
|
Sign up to set email alerts
|

Electrochemical machining of molybdenum

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
2
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 10 publications
(2 citation statements)
references
References 22 publications
0
2
0
Order By: Relevance
“…8G,H). When the current density reached 30 A/ cm 2 , the oxygen-rich region was broken and the oxy- gen content increased, attributed to the stronger electrolytic effect and anodic oxygen evolution [35][36][37]. Unlike surface of G1 at 1 A/cm 2 , there was no intergranular corrosion on the surface of G2 at low current density.…”
Section: Ecm Experimentsmentioning
confidence: 99%
“…8G,H). When the current density reached 30 A/ cm 2 , the oxygen-rich region was broken and the oxy- gen content increased, attributed to the stronger electrolytic effect and anodic oxygen evolution [35][36][37]. Unlike surface of G1 at 1 A/cm 2 , there was no intergranular corrosion on the surface of G2 at low current density.…”
Section: Ecm Experimentsmentioning
confidence: 99%
“…1c), which emerged in 2003/2004, 31,32 represents a more attractive laboratory setup for investigation of ECM fundamentals because it simultaneously enables a near-ECM environment, allows for use of almost all common measurement techniques, and reduces the subsequent analysis efforts required. [8][9][10][11]22,[33][34][35][36][37] Because of the θ-type cross-section, there are two channels, which serve as the inlet and the outlet, to enable realization of fast electrolyte flow. Importantly, the small WE area determined by the end mouth of the θ-capillary and the narrow WEz E-mail: wdliu@cauc.edu.cn to-CE gap allows polarization to the high current density range when using a potentiostat.…”