“…Figure S5d shows that the spectral peaks associated with -OH, N–H, and others disappeared (505, 791, 1064, 1410, 1927, and 3210 cm –1 ), while new peaks appeared at 3438, 1628, 983, 865, 655, and 474 cm –1 after 100 min of SSR at 500 °C. The peaks at 3438/1628, 983/865, 655, and 474 cm –1 are attributable to metal orthophosphate stretching vibrations, MoO/Mo–O–Mo, P–O, and metal-M-O (Pd and Ni) bonds, respectively. ,− No absorption peaks of ammonium compounds were detected after calcination (Figure S5d), suggesting that they were evaporated and that the Pd 6% Ni-P 2 O 5 /MoO 3 HPHS was produced.…”