“…Successive discharges at high frequencies produce many randomly placed overlapping craters. The shape and the depth of the craters, which determine the surface roughness of the rolls, depend mainly on the operational parameters such as discharge current, discharge duration, and polarity used [4][5][6]. Compared with traditional shot blasting texturing, EDT allows higher number of peaks at constrained average surface roughness, which can be obtained in a higher repeatability.…”