Ein thermisch induzierter Spinübergang an einem Eisen(II)‐Komplex mit einer 70 K breiten Hystereseschleife

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
27
0

Year Published

2009
2009
2019
2019

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 56 publications
(27 citation statements)
references
References 36 publications
(14 reference statements)
0
27
0
Order By: Relevance
“…K to a value of 2.89 cm 3 Kmol -1 at 20 K. The susceptibility data above 20 K can be fitted very well with the Curie-Weiss law (χ M = C/(T -Θ )) with the parameters Θ = -7.5 K and C = 3.50 cm…”
Section: Magnetic Propertiesmentioning
confidence: 74%
See 4 more Smart Citations
“…K to a value of 2.89 cm 3 Kmol -1 at 20 K. The susceptibility data above 20 K can be fitted very well with the Curie-Weiss law (χ M = C/(T -Θ )) with the parameters Θ = -7.5 K and C = 3.50 cm…”
Section: Magnetic Propertiesmentioning
confidence: 74%
“…Upon cooling, the χ M T product decreases from a value of 3.32 cm 3 Kmol -1 at 300 K to a value of 1.33 cm 3 Kmol -1 at 20 K. The room temperature value is in the region typical for an iron(II) HS complex. The temperature-dependent decrease of the χ M T product is an indication for significantly stronger antiferromagnetic interactions compared to 2.…”