Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts

Abstract: In this study, the effects of the post-ultraviolet-curing process on the flexural, absorptive, and morphological properties of poly(lactic acid) specimens produced using a fused deposition modelling technique 3D printer were experimentally investigated. In this direction, 15, 30, 45, and 60 min post-UV-curing processes were applied to poly(lactic acid) three-point bending and absorption specimens produced at 190 and 200 °C. Three-point bending tests and morphological analyses were applied after the post-ultrav… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
5
0

Year Published

2023
2023
2023
2023

Publication Types

Select...
2

Relationship

1
1

Authors

Journals

citations
Cited by 2 publications
(5 citation statements)
references
References 73 publications
0
5
0
Order By: Relevance
“…The findings of this study are consistent with the study conducted by Hsueh et al [36], and the 60-min post-UV-curing process causes a decrease in the mechanical properties of PLA parts. In the study by Akderya [38], the effects of the post-UV-curing process applied between 15-60 minutes on the flexural and absorptive properties of PLA parts were investigated. In accordance with this study, it is seen that the mechanical properties of the specimens applied 30-min post-UV-curing have the highest value.…”
Section: Resultsmentioning
confidence: 99%
See 3 more Smart Citations
“…The findings of this study are consistent with the study conducted by Hsueh et al [36], and the 60-min post-UV-curing process causes a decrease in the mechanical properties of PLA parts. In the study by Akderya [38], the effects of the post-UV-curing process applied between 15-60 minutes on the flexural and absorptive properties of PLA parts were investigated. In accordance with this study, it is seen that the mechanical properties of the specimens applied 30-min post-UV-curing have the highest value.…”
Section: Resultsmentioning
confidence: 99%
“…As a result of the emergence of the photo-oxidative degradation process with the effect of UVirradiation, an irregular, uneven, and variable adhesion success has emerged between the printing fibres. The biodegradable structure of PLA is triggered by the emergence of the photo-oxidative degradation process, and the phenomenon adversely affects the adhesion success of printing fibres that form the material structure [38,50]. In addition, the specimens exposed to the post-UV-curing process for 30 minutes have the highest peak force and energy values.…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“…In this study, a new method for UV light measurement was developed. In this method, 3D printable filaments, which are a product of Polylactic Acid (PLA) Photochromic materials that change color under UV light, were used [6]. Although PLA has high mechanical strength and superior thermal processability, using it pure is far from functional [7].…”
Section: Introductionmentioning
confidence: 99%