2010
DOI: 10.1109/tmag.2009.2034537
|View full text |Cite
|
Sign up to set email alerts
|

Effects of Magnetic Phase on the ECT Signal in the SG Tubes

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2011
2011
2011
2011

Publication Types

Select...
1
1

Relationship

2
0

Authors

Journals

citations
Cited by 2 publications
(2 citation statements)
references
References 4 publications
0
2
0
Order By: Relevance
“…The existence of MP in a SGT was verified from a retired SGT (Inconel 600) of Kori-1 NPP in Korea by showing a permanent magnet attached to the fragment of a SGT containing the MP [1]. The axial defects in a SGT can be detected by conventional ECT, but the CDs and CMPs are very difficult to detect.…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…The existence of MP in a SGT was verified from a retired SGT (Inconel 600) of Kori-1 NPP in Korea by showing a permanent magnet attached to the fragment of a SGT containing the MP [1]. The axial defects in a SGT can be detected by conventional ECT, but the CDs and CMPs are very difficult to detect.…”
Section: Methodsmentioning
confidence: 99%
“…The materials used for SGT are Inconel alloys, which are non-magnetic and have good corrosion-resistance. On the other hand, MPs and defects are partly generated in the SGT due to the high temperatures and stresses because the temperature and pressure of water in SGTs are very high due to nuclear fission [1]. The temperature and pressure is approximately 280 o C and 15.5 MPa, respectively.…”
Section: Introductionmentioning
confidence: 99%