Effects of Au and F co-modification by thermal shock method on the photocatalytic activity of ZnO

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(4 citation statements)
references
References 42 publications
0
4
0
Order By: Relevance
“…The peak at 82 eV was assigned to the Au 4f7/2 of Au 0 , while the peaks at 87 and 91 eV were assigned to the Au 4f5/2 of Au 3+ (Fig. 5(f)) (Sylvestre et al, 2004;Dillip et al, 2020;Tran Vu et al, 2021). The optical absorption properties of the samples are shown in Fig.…”
Section: Resultsmentioning
confidence: 97%
“…The peak at 82 eV was assigned to the Au 4f7/2 of Au 0 , while the peaks at 87 and 91 eV were assigned to the Au 4f5/2 of Au 3+ (Fig. 5(f)) (Sylvestre et al, 2004;Dillip et al, 2020;Tran Vu et al, 2021). The optical absorption properties of the samples are shown in Fig.…”
Section: Resultsmentioning
confidence: 97%
“…This means that this MB solution is stable under UV irradiation, unlike those in other works that reported a considerable effect of UV light on MB (% deg > 5); 4,[36][37][38] these results could be due to the highpower lamps used during research. Other studies do not report photolysis effects in their MB degradation results; 12,19,25,[39][40][41][42] even when photolysis is measured, their reported degradation percentages are not reliable and comparison with other catalysts is not possible. On the other hand, the adsorption of MB onto ZnO and Au/ZnO surfaces was carried out as expected.…”
Section: Photocatalytic Activitiesmentioning
confidence: 97%
“…For example, some works used organic ligands as thiol and amino molecules; 6,7 however, the main disadvantage was that, in order to remove the ligand, an additional process involving high temperatures was needed. Other ‘facile’ chemical methods need long stirring times (12 and 5 h), 8‐10 hazardous reducing agents (such as hydrazine hydrate and NaBH 4 ) 11‐17 or high annealing temperatures (above 450 °C) to obtain ZnO nanostructures, and Au deposition or the removal of any organic residues 16,18‐25 . Even photochemical processes lost their simplicity due long irradiation times (180, 600, and 720 min) 26‐28 .…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation