Effect of wire mesh interlayer in explosive cladding of dissimilar grade aluminum plates

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 22 publications
(5 citation statements)
references
References 19 publications
0
5
0
Order By: Relevance
“…The observed increase in hardness value within the deformed area can be attributed to dynamic collisions, [45] the presence of ultrafine grains, [31] and the significant levels of plastic deformation resulting from work hardening processes at the weld interface. [46,47] The recrystallization process arises from the impact phenomenon occurring between two mating surfaces at high temperature and pressure. [37,48] The observed fluctuations in hardness value on both the JIS G 5501 and JIS G 5502 sides can be attributed to the random dispersion of graphite flakes/nodules within the material.…”
Section: Right Limitmentioning
confidence: 99%
“…The observed increase in hardness value within the deformed area can be attributed to dynamic collisions, [45] the presence of ultrafine grains, [31] and the significant levels of plastic deformation resulting from work hardening processes at the weld interface. [46,47] The recrystallization process arises from the impact phenomenon occurring between two mating surfaces at high temperature and pressure. [37,48] The observed fluctuations in hardness value on both the JIS G 5501 and JIS G 5502 sides can be attributed to the random dispersion of graphite flakes/nodules within the material.…”
Section: Right Limitmentioning
confidence: 99%
“…By using the laws of conduction and convection, the changed kinetic energy in the region between the flyer plate and the interlayer is translated into thermal energy and used to produce plastic deformation (Eqn. 7) [5]. With the remaining kinetic energy, the flyer-interlayer clad then collides with the base plate, enhancing the deformation work (Eqn.…”
Section: Interlayer and Kinetic Energy Utilizationmentioning
confidence: 99%
“…The kinetic energy utilization and deformation work performed in conventional two-layer cladding are enhanced by introducing a compatible interlayer [5]. The introduction of an interlayer doubles the area of collision, and thereby, the formation of a melted layer across the conventional clad interface is nullified or with a slender presence.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Hybrid composites exhibit superior mechanical properties viz., higher hardness, fracture toughness, fatigue resistance and creep resistance [1]. In addition, these composites show higher corrosion and wear resistance and thereby, are excellent replacement for conventional metals and alloys [2]. The choice of processing condition, fabrication process and the choice of reinforcement significantly improve the mechanical and metallurgical properties of hybrid composites.…”