Effect of Sb Modification and B Refinement on the Microstructure and Properties of as-Cast Al–7Si–0.35Mg Alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2

Citation Types

0
2
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 34 publications
0
2
0
Order By: Relevance
“…The beneficial effect of Sb is also reported in 319 alloys [52,56]. Its optimum amount might vary considerably depending on alloy composition and casting conditions, ranging from 0.009wt% [56] to 0.6wt% [53]. Likewise, bismuth (Bi) exerts the same effect on eutectic morphology and does not increase porosity.…”
Section: Modifiers Of the Eutectic Morphologymentioning
confidence: 96%
See 1 more Smart Citation
“…The beneficial effect of Sb is also reported in 319 alloys [52,56]. Its optimum amount might vary considerably depending on alloy composition and casting conditions, ranging from 0.009wt% [56] to 0.6wt% [53]. Likewise, bismuth (Bi) exerts the same effect on eutectic morphology and does not increase porosity.…”
Section: Modifiers Of the Eutectic Morphologymentioning
confidence: 96%
“…Antimony has a slightly different action, producing a lamellar morphology instead of fibrous [3,52]. Cai et al attributed its modification effect to the precipitation AlSb compounds during solidification, which were absorbed in the growth front of the eutectic Si, inhibiting growth and thus refining Si particles [53]. It does not increase porosity like strontium.…”
Section: Modifiers Of the Eutectic Morphologymentioning
confidence: 99%