Abstract: Aims:To evaluate the effect of the addition of MgO, ZrO2, ZnO nanoparticles in different concentration to acrylic based soft liner on candida Albicans adhesion. Materials and methods: acrylic-based soft-liner samples were prepared (10 X10 X 2mm dimension) by addition MgO, ZrO2, ZnO nanoparticles in 0.25, 0.5, 1, 2, 4 % by weight concentration to the monomer resin, the samples were immersed in Candida Albicans suspension for 1 hour then washed and dried, the microorganism were fixed and stained by crystal viole… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(3 citation statements)
references
References 19 publications
(23 reference statements)
0
3
0
Order By: Relevance
“…After that, the wax blocks were placed in a dental stone with the metal spacer (10mm, 10mm, and 3mm in dimensions) dividing two wax blocks for a soft-liner film. The acrylic resin mold was created after the wax blocks were eliminated (7,8). The CAD/CAM-based PMMA polymer (NHT, Latvia) was used to prepare the acrylic sample blocks by CAD/CAM machine (imes-icore, 250i, Germany) as shown in Fig.…”
Section: Methodsmentioning
confidence: 99%
“…After that, the wax blocks were placed in a dental stone with the metal spacer (10mm, 10mm, and 3mm in dimensions) dividing two wax blocks for a soft-liner film. The acrylic resin mold was created after the wax blocks were eliminated (7,8). The CAD/CAM-based PMMA polymer (NHT, Latvia) was used to prepare the acrylic sample blocks by CAD/CAM machine (imes-icore, 250i, Germany) as shown in Fig.…”
Section: Methodsmentioning
confidence: 99%
“…The wax blocks were then invested in a dental stone with metal spacer dimensions (10mm, 10mm, and 3mm) separating two wax blocks for a resilient liner film. After the wax was eliminated, the mold for acrylic resin was created (6,7). The acrylic resin (Procryla, Presidental Dental, Germany) was mixed and packed on both sides of the spacer Fig.…”
Section: Specimens Preparationmentioning
confidence: 99%
“…A total of 30 samples were made; 15 specimens for hardness measurement with dimensions (30mm and 3mm in diameter and thickness respectively) (6,7) and 15 specimens for surface roughness measurement with dimensions (10mm length, 10mm width, and 3mm thickness) (7,8). modeling wax with specific measurements for each test was invested in a dental stone for mold creation Fig.…”
Section: Specimens Processingmentioning
confidence: 99%