Effect of cooling temperature on the microstructure and corrosion behavior of X80 pipeline steel

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

0
11
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 15 publications
(11 citation statements)
references
References 5 publications
0
11
0
Order By: Relevance
“…Previous research shows that the finishing rolling temperature and beginning quick cooling temperature, i.e., relaxation time, are very important in determining the volume fractions of ferrite and bainite [ 12 , 13 ]. The C content in undercooled austenite increases as the ferrite transformation and amount increases; simultaneously, the subsequent rapid cooling rate affects the microstructure and mechanical properties of the bainite [ 19 ]. As a result, the bainite change in strength and plasticity causes the variation in the strength and plasticity of the F/B dual-phase pipeline steels.…”
Section: Introductionmentioning
confidence: 99%
“…Previous research shows that the finishing rolling temperature and beginning quick cooling temperature, i.e., relaxation time, are very important in determining the volume fractions of ferrite and bainite [ 12 , 13 ]. The C content in undercooled austenite increases as the ferrite transformation and amount increases; simultaneously, the subsequent rapid cooling rate affects the microstructure and mechanical properties of the bainite [ 19 ]. As a result, the bainite change in strength and plasticity causes the variation in the strength and plasticity of the F/B dual-phase pipeline steels.…”
Section: Introductionmentioning
confidence: 99%
“…Controlling the cooling process during their production can optimize the microstructure and mechanical properties of steel plates. [1] The traditional quenching method involves transferring a high-temperature ultrathick plate from the furnace to the water tank and accelerating the heat exchange by stirring the coolant. However, the uneven and gentle convection conditions result in low cooling capacity and poor uniformity.…”
Section: Introductionmentioning
confidence: 99%
“…That has driven the specialists to investigate their appropriateness for various structural and constructional purposes (Katiyar et al 2019). Though plenty of research articles were published concerning a generally excellent blend of mechanical properties in DP steels (Karimi et al 2017;Basantia et al 2021;Bilal et al 2019;Fereiduni and Ghasemi Banadkouki 2014;Kumar et al 2019;Shahzad et al 2018;Xiong et al 2019;Zhao et al 2019;Zhu 2019), further examinations are important to discover the impact of phase constituents on the corrosion resistance properties (Bignozzi et al 2020;Gürkan Aydın 2019;Ma et al 2020;Prabhu et al 2020a, b;Zhang et al 2020).…”
Section: Introductionmentioning
confidence: 99%