2004
DOI: 10.4012/dmj.23.53
|View full text |Cite
|
Sign up to set email alerts
|

Determination of the Fabricating Conditions for the Preferable Marginal and Internal Adaptation of the Mica Crystal Castable Ceramic Crown

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
4
0
3

Year Published

2005
2005
2021
2021

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 9 publications
(7 citation statements)
references
References 12 publications
0
4
0
3
Order By: Relevance
“…There are two methods to measure the deformation of crowns and FPDs. One is to measure the gap between the master die and the restoration [21][22][23][24][25][26] ; the other is to read the three-dimensional coordinates on the reference plane using a three-dimensional coordinate measuring machine or the coordinates at the points defined on the restoration, and then perform vector analysis 27) . The former method is easy in terms of visualizing marginal discrepancies, but it is inconvenient for the measurement of threedimensional helical deformations.…”
Section: Measurement and Analysis Methodsmentioning
confidence: 99%
“…There are two methods to measure the deformation of crowns and FPDs. One is to measure the gap between the master die and the restoration [21][22][23][24][25][26] ; the other is to read the three-dimensional coordinates on the reference plane using a three-dimensional coordinate measuring machine or the coordinates at the points defined on the restoration, and then perform vector analysis 27) . The former method is easy in terms of visualizing marginal discrepancies, but it is inconvenient for the measurement of threedimensional helical deformations.…”
Section: Measurement and Analysis Methodsmentioning
confidence: 99%
“…In light of this clinically acceptable range, the CAD/CAM crowns fabricated in this study were considered clinically safe and applicable [18][19][20][21][22][23][24] .…”
Section: Influence Of Step-overmentioning
confidence: 99%
“…Considera-se, porém, que clinicamente a espessura do cimento é muito menor que a testada, tendo no máximo 120 µm (Ukon et al, 2004;Freire et al, 2016). A espessura de 0,5mm para amostras do grupo controle dos Cimentos foi escolhida, pois, apesar de ser bem maior do que a linha de cimentação produzida pelo cimento durante a cimentação dos laminados cerâmicos, essa seria a espessura mínima capaz de permitir colher resultados confiáveis para analise da cor das amostras (Silami et al, 2016;.…”
Section: Discussionunclassified
“…Os valores de linha de cimentação mensurados neste estudo, variaram de 24µm à 85µm, sem diferença entre os cimentos resinoso utilizados na pesquisa. Para cimentação realizada com cimentos resinosos esses valores são considerados "clinicamente aceitáveis", podendo a linha de cimentação medir até 120µm(Ukon et al, 2004, Freire et al, 2016.Discussão | 109 translucidez nos grupos restaurados quando usada a ciclagem termomecânica como um método de envelhecimento. A simplificação da cimentação com cimentos autoadesivos, visando melhorar a sensibilidade técnica é uma inquestionável conquista.…”