Determination of high temperature mechanical properties of thermal barrier coatings by nanoindentation

Abstract: A nanoindentation method is employed to measure the high temperature mechanical properties, including hardness H, Young's modulus E and fracture toughness K c , of 8YSZ (ZrO 2 z8 wt-%Y 2 O 3 ) thermal barrier coatings (TBCs) under as sprayed condition and after subjecting them to thermal oxidation. The tests are conducted on the surfaces of YSZ coatings at temperatures of 250 and 450uC. The expressions for indentation H and E are deduced analytically, and the influence of testing temperature and thermal oxidat… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
18
0

Year Published

2017
2017
2022
2022

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 33 publications
(18 citation statements)
references
References 20 publications
0
18
0
Order By: Relevance
“…The crack length could be measured. Formula (1) reflects the relationship of fracture toughness and crack length according to the Nihhara relation [41]:…”
Section: Propertiesmentioning
confidence: 99%
“…The crack length could be measured. Formula (1) reflects the relationship of fracture toughness and crack length according to the Nihhara relation [41]:…”
Section: Propertiesmentioning
confidence: 99%
“…e elastic modulus and maximum depth of the indentation of the base material are selected as the fundamental quantity. Π theorem is applied to nondimensionalize equations (12) and (13), and the following equations can be obtained:…”
Section: Substrate Effect In Indentation Of In Coating and Dimensionlmentioning
confidence: 99%
“…In the numerical simulation of this study, fixed maximum depth of the indentation (equal to that in the indentation test) is taken, and equations (12) and (13) can be expressed as…”
Section: Substrate Effect In Indentation Of In Coating and Dimensionlmentioning
confidence: 99%
See 1 more Smart Citation
“…3) It is to utilize the indentation method directly to evaluate HT modulus of coatings at temperatures below 1000 ℃ [16][17][18]. However, the drawback stems from the oxidation, erosion, and stiffness degradation of the indenter at HT that affect deeply the measurements [19,20].…”
Section: Introductionmentioning
confidence: 99%