Critical current density of Ag-sheathed (Bi,Pb) 2223 tapes produced by various thermo-mechanical treatment patterns

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

1998
1998
2012
2012

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 6 publications
(2 citation statements)
references
References 10 publications
0
2
0
Order By: Relevance
“…The degree of the texturing was evaluated by the full width at half maxi-mum (FWHM) along the rolling direction of the (0 0 14) pole intensity normal to the rolling plane [22]. Transversal crosssection images of tapes were observed on a Nova 400 Nano-SEM in the backscattered electron (BSE) imaging mode.…”
Section: Methodsmentioning
confidence: 51%
“…The degree of the texturing was evaluated by the full width at half maxi-mum (FWHM) along the rolling direction of the (0 0 14) pole intensity normal to the rolling plane [22]. Transversal crosssection images of tapes were observed on a Nova 400 Nano-SEM in the backscattered electron (BSE) imaging mode.…”
Section: Methodsmentioning
confidence: 51%
“…In previous studies it has been proven that a sufficient combination of heat treatment and mechanical deformation (flat rolling or pressing) can improve the J c of Bi-2223/Ag tapes [4][5][6][7]. The mechanical deformation was found to improve the alignment of Ag/Bi 1.8 Pb 0.4 Sr 2 Ca 2.2 Cu 3 O 10−x (Bi-2223) grains in the tapes [8][9][10], to increase the HTSC core density [11,12] and to facilitate greater conversion of precursor powder to the 2223 phase in the tapes [13].…”
Section: Introductionmentioning
confidence: 99%