2008
DOI: 10.1007/s10853-008-2725-8
|View full text |Cite
|
Sign up to set email alerts
|

Crack growth in ultrafine-grained AA6063 produced by equal-channel angular pressing

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
16
0
5

Year Published

2009
2009
2015
2015

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 54 publications
(21 citation statements)
references
References 19 publications
0
16
0
5
Order By: Relevance
“…Additionally, striations are clearly visible. Such signs of "micro-damage" have also been observed for other ECAP-processed aluminum alloys [16]. They were interpreted as the severely strain-hardened material is not being able to compensate the stresses at the crack tip by deforming plastically.…”
Section: Fatigue Crack Surface Analysismentioning
confidence: 55%
See 1 more Smart Citation
“…Additionally, striations are clearly visible. Such signs of "micro-damage" have also been observed for other ECAP-processed aluminum alloys [16]. They were interpreted as the severely strain-hardened material is not being able to compensate the stresses at the crack tip by deforming plastically.…”
Section: Fatigue Crack Surface Analysismentioning
confidence: 55%
“…These investigations show the well-known effect of the grain or particle size on the fatigue crack growth. The grain refinement through ECAP leads to a minimized amount of crack deflection and roughness-induced crack closure, which results in higher crack propagation rates and, therefore, in minor thresholds [11][12][13][14][15][16][17][18]. In reinforced materials, particle sizes larger than 2-5 µm have a contrary effect on crack propagation: by increasing crack deflection and roughness-induced crack closure, crack propagation rates are lowered [19][20][21][22][23][24].…”
Section: Introductionmentioning
confidence: 99%
“…Zunahmen der Fließgrenze von circa 135% bei EN AW-7075 bis circa 400% bei EN AW-1100 gegenüber weichen, normalkörnigen Zuständen werden dargestellt. Aluminiumlegierungen im ultrafeinkörnigen Zustand zeigen neben einer Steigerung der Festigkeit eine erhöhte Risswachstumsneigung [9] während die Rissinitiierung verzögert ist [10].…”
Section: Motivationunclassified
“…Die Versuche wurden DK-geregelt bei konstanten Spannungsverhältnissen R = K min /K max in einer Resonanzprüfmaschine der Firma RUMUL durchgeführt. Die Prozedur zur Ermittlung des Schwellwertes DK th ist in [12] beschrieben. …”
Section: Untersuchungen Des Rissfortschrittsunclassified