Coupling of breath figure method with interfacial polymerization: Bottom-surface functionalized honeycomb-patterned porous films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
15
0

Year Published

2017
2017
2021
2021

Publication Types

Select...
7
1

Relationship

2
6

Authors

Journals

citations
Cited by 33 publications
(15 citation statements)
references
References 30 publications
0
15
0
Order By: Relevance
“…The simplest (and an extremely useful) method of characterization of micro-rough surfaces is based on the measurement of the apparent contact angle [ 32 , 33 , 34 , 164 ]. A detailed study of the apparent contact angles inherent for honeycomb, porous surfaces arising from breath-figure self-assembly was reported in [ 165 , 166 , 167 ]. It was demonstrated that honeycomb surfaces produced by breath-figure self-assembly demonstrate a pronounced heterogeneous (air-trapping) Cassie–Baxter wetting regime [ 79 , 168 , 169 , 170 ].…”
Section: Characterization Of Patterns Obtained With Breath-figure mentioning
confidence: 99%
“…The simplest (and an extremely useful) method of characterization of micro-rough surfaces is based on the measurement of the apparent contact angle [ 32 , 33 , 34 , 164 ]. A detailed study of the apparent contact angles inherent for honeycomb, porous surfaces arising from breath-figure self-assembly was reported in [ 165 , 166 , 167 ]. It was demonstrated that honeycomb surfaces produced by breath-figure self-assembly demonstrate a pronounced heterogeneous (air-trapping) Cassie–Baxter wetting regime [ 79 , 168 , 169 , 170 ].…”
Section: Characterization Of Patterns Obtained With Breath-figure mentioning
confidence: 99%
“…A broad range of absorption was observed between 250 and 300 nm for PS‐CHO with an absorbance maximum at 255–260 nm due to the presence of aromatic groups in each of its repeating units. Whereas in case of polystyrene showed absorption maximum at 265 nm …”
Section: Resultsmentioning
confidence: 96%
“…For the comparison, PEDOT:PSS MEP film was fabricated via similar process using PS HCP film as a template. PS HCP film was fabricated using the BF method . Briefly, a 250 mg of PS was dissolved in 5 mL of THF.…”