2019
DOI: 10.1007/s12598-019-01234-1
|View full text |Cite
|
Sign up to set email alerts
|

Corrosion resistance of Mg(OH)2/Mg–Al-layered double hydroxide coatings on magnesium alloy AZ31: influence of hydrolysis degree of silane

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
15
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 56 publications
(17 citation statements)
references
References 57 publications
0
15
0
Order By: Relevance
“…The surface roughness (R a ) was tested by a Mg alloy surface had occurred. 33,34 A significant rise in peak intensity could be seen at 2920 and 2850 cm À1 , which corresponded to the asymmetric vibration peak and the symmetric stretching vibration peak of CH 2 , 35,36 respectively. It was due to the increase of chain length, which enhanced the density of CH 2 in the dual-component silane films.…”
Section: Characterizationmentioning
confidence: 94%
See 1 more Smart Citation
“…The surface roughness (R a ) was tested by a Mg alloy surface had occurred. 33,34 A significant rise in peak intensity could be seen at 2920 and 2850 cm À1 , which corresponded to the asymmetric vibration peak and the symmetric stretching vibration peak of CH 2 , 35,36 respectively. It was due to the increase of chain length, which enhanced the density of CH 2 in the dual-component silane films.…”
Section: Characterizationmentioning
confidence: 94%
“…R ct reflected the difficulty of charge transfer through the interface between the electrode and the electrolyte in the electrode process. 33 The value of R ct was related to the corrosion rate. The larger the value, the harder the charge transfer process.…”
Section: Characterizationmentioning
confidence: 99%
“…As the PMTMS is more durable and acts as a physical barrier to prevent the corrosive solution from attacking, the composite coating of MAO/PMTMS shows greater corrosion resistance than the coating of MAO. However, the PMTMS coating is susceptible to swelling and peeling off [205].…”
Section: N-doping Gqds For Raising Corrosion Preventionmentioning
confidence: 99%
“…In the past 5 years, new strategy was proposed to protect corrosive metals, that is preparing non-metallic protective layer on the surface of metal substrates [5][6][7][8][9][10]. So far, hydroxides, graphene, and organic materials on metal substrates have been fabricated and investigated for coating materials [5,6,[11][12][13][14].…”
Section: Introductionmentioning
confidence: 99%