Corrosion inhibition of carbon steel by dipotassium hydrogen phosphate in alkaline solutions with low chloride contamination

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
20
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 45 publications
(22 citation statements)
references
References 47 publications
2
20
0
Order By: Relevance
“…Generally, the large concentrations improve solution conductivity and provide sufficient reactants on the interfaces to expedite the corrosion process. [ 74 ] 2)Diffusion rates of ions/oxygen gases: the corrosion reaction actually involves the diffusion of different ions and oxygen gases on the surfaces of metal substrates, while the faster diffusion rates always bring forth the severer corrosion. [ 75,76 ] Employing vigorous stirring for the accelerated convection is the commonly used method to promote diffusion rates, which can be used to shorten the reaction time of corrosion engineering and enhance the homogeneity of target materials. 3)Surrounding atmosphere: herein, oxygen corrosion is adopted as an example, which can only happen in the oxygen‐containing atmosphere.…”
Section: Description Of Corrosion Engineeringmentioning
confidence: 99%
“…Generally, the large concentrations improve solution conductivity and provide sufficient reactants on the interfaces to expedite the corrosion process. [ 74 ] 2)Diffusion rates of ions/oxygen gases: the corrosion reaction actually involves the diffusion of different ions and oxygen gases on the surfaces of metal substrates, while the faster diffusion rates always bring forth the severer corrosion. [ 75,76 ] Employing vigorous stirring for the accelerated convection is the commonly used method to promote diffusion rates, which can be used to shorten the reaction time of corrosion engineering and enhance the homogeneity of target materials. 3)Surrounding atmosphere: herein, oxygen corrosion is adopted as an example, which can only happen in the oxygen‐containing atmosphere.…”
Section: Description Of Corrosion Engineeringmentioning
confidence: 99%
“…The pH value of IWP is 9.64 because it contains alkaline oxides such as iron and calcium oxides. The CR can be slowed down in alkaline mediums due to the formation of a protective passive film of insoluble metal hydroxides . However, the presence of copolymer on the IWP surface reduced the pH value of the COIW to 6.06.…”
Section: Resultsmentioning
confidence: 99%
“…The CR can be slowed down in alkaline mediums due to the formation of a protective passive film of insoluble metal hydroxides. [37,38] However, the presence of copolymer on the IWP surface reduced the pH value of the COIW to 6.06. This may be due to the presence of the copolymer in the protonation form.…”
Section: Evaluation Of the Pigmentsmentioning
confidence: 99%
“…For instance, the majority of ship pipeline is fabricated by LCS 3 . However, LCS has weak corrosion resistance 4 . To improve reliability and durability of ship LCS pipeline, a large number of technologies have been employed for LCS pipes, such as electrogalvanizing, hot-dip galvanizing, powder zinc impregnation, rubber-coated pipes, and fiberglass pipes 5 8 .…”