Corrosion Fatigue Behavior of High Strength Stainless Steel Manufactured by Three Different Melting Processes.

Abstract: The corrosion fatigue tests in city water were carried out on precipitation hardening stainless steel, SUS630, variously heat treated (H1075, H1025, and H900), which was manufactured by three different melting processes (air, double and triple melting process). The results obtained are as follows.The corrosion fatigue strength of all H1075 specimens manufactured by three melting processes decreased compared with fatigue strength in air. The triple melted H1075 specimen showed the highest value of corrosion fat… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Year Published

2016
2016
2016
2016

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
references
References 0 publications
0
0
0
Order By: Relevance