1999
DOI: 10.1016/s0924-4247(99)00008-4
|View full text |Cite
|
Sign up to set email alerts
|

Chemical tapering of polymer optical fibre

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
71
0

Year Published

2006
2006
2022
2022

Publication Types

Select...
7
2
1

Relationship

0
10

Authors

Journals

citations
Cited by 114 publications
(74 citation statements)
references
References 9 publications
0
71
0
Order By: Relevance
“…To fabricate the POF SERS sensor, we used the etching method [42] to prepare the POF tip with a diameter of 2 μm-3 μm. Then several drops of gold nanorods colloids were placed directly on the POF tip and dried naturally.…”
Section: Optical Fiber Sers Sensorsmentioning
confidence: 99%
“…To fabricate the POF SERS sensor, we used the etching method [42] to prepare the POF tip with a diameter of 2 μm-3 μm. Then several drops of gold nanorods colloids were placed directly on the POF tip and dried naturally.…”
Section: Optical Fiber Sers Sensorsmentioning
confidence: 99%
“…Then in the first sample, labeled as LM-1 in table 1, the outer jacket is simply stripped off in an approximately 2 cm length and the fiber tip polished. The second sample, labeled as LM-2 in table 1, keeps approximately the same length of exposed fiber, but the fiber diameter is homogeneously reduced by chemical etching with pure acetone to a diameter of 880 µm [16][17][18]. With this procedure, cladding and part of the core of the fiber distal end is removed.…”
Section: Transducers Fabrication and Experimental Setupmentioning
confidence: 99%
“…The fiber core outer diameter is 980 µm. It has been previously reported that the PMMA optical fiber can be bi-conically tapered at the fiber tip using 60% acetone, 20% MIBK and 20% distilled water (AMD solution) [20]. In our work this method has been modified to carry out etching of core at the centre of fiber.…”
Section: A Preparation Of Sensing Elementmentioning
confidence: 99%