Characterization and Thermo-stability of Alkylated Polyparaphenylene

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2009
2009
2023
2023

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(3 citation statements)
references
References 12 publications
0
3
0
Order By: Relevance
“…It could also bring the optimal operating temperature range down to lower temperatures opening up the operating temperature window of the individual oxide [ 32 , 95 ]. Manipulation of the polymer structure via substitution or addition reactions, i.e., functionalisation of the polymer, is also known to alter the temperature of thermal degradation [ 202 , 203 , 204 ]. This effect is also observed when polymers are doped [ 205 ].…”
Section: Discussionmentioning
confidence: 99%
See 1 more Smart Citation
“…It could also bring the optimal operating temperature range down to lower temperatures opening up the operating temperature window of the individual oxide [ 32 , 95 ]. Manipulation of the polymer structure via substitution or addition reactions, i.e., functionalisation of the polymer, is also known to alter the temperature of thermal degradation [ 202 , 203 , 204 ]. This effect is also observed when polymers are doped [ 205 ].…”
Section: Discussionmentioning
confidence: 99%
“… Reported temperature ranges of organic polymers ( A ) and oxides ( B ) in air as a function of temperature (K). ( A ) PPP [ 202 ], PANI (Base) [ 206 ], PPy [ 207 ], PEDOT [ 208 ], PANI (unoxidised) [ 209 ], PEDOT:PSS [ 208 ], PEDOT:PSS (doped) [ 208 , 210 ], PPy (doped) [ 207 ], PANI (doped) [ 206 ], and PVA [ 211 ]. ( B ) TiO 2 [ 212 ], In 2 O 3 :Ge [ 80 ], SrTiO 3 [ 213 ], BiSrCoO [ 80 ], Ca 3 Co 4 O 9 [ 214 ], ZnO [ 23 ], TiO 2 /SrTiO 3 –biphase [ 215 ], NaCoO 2 [ 24 ], CaMnO 3 [ 216 ], and MnO 2 [ 217 ].…”
Section: Discussionmentioning
confidence: 99%
“…The reduction in IDT of aromatic polymers by substitution of alkyl group that is susceptible for degradation is known in the literature. For example, significant deterioration of thermal stability of poly(p-phenylene) after its substitution with thermally labile iso-propyl and iso-amyl groups is reported [27]. In case of PILs bearing a particular substituent but with varying anion, thermal stability increased with the order of anions as HFB̄oIrBF 4̄o Tf 2 N̄.…”
Section: Thermal Stability Of Pilsmentioning