Carbon Nanofiber Synthesis within 3-Dimensional Sintered Nickel Microfibrous Matrices: Optimization of Synthesis Conditions

Abstract: This study focuses on the process of optimization for carbon nanofiber synthesis at the exterior and the interior of 3-dimensional sintered nickel microfibrous networks. Synthesis of carbon nanofibers (CNF) by catalytic decomposition of acetylene (ethyne) was conducted at atmospheric pressure and short reaction times (10 min). Two factors evaluated during the study were (a) CNF quality (observed by SEM and Raman spectroscopy) and (b) rate of reaction (gravimetrically measured carbon yield). Independent optimiz… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2016
2016
2020
2020

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 73 publications
0
1
0
Order By: Relevance
“…CNFs synthesis was successfully achieved on a 50 mm nickel wire with three different synthesis temperatures (500 C, 600 C and 700 C). The surface morphology proved to be highly dependent on the synthesis temperature [25]. The thickness of the layer varies mainly with the synthesis duration and temperature.…”
Section: Cnfs Layer Synthesismentioning
confidence: 99%
“…CNFs synthesis was successfully achieved on a 50 mm nickel wire with three different synthesis temperatures (500 C, 600 C and 700 C). The surface morphology proved to be highly dependent on the synthesis temperature [25]. The thickness of the layer varies mainly with the synthesis duration and temperature.…”
Section: Cnfs Layer Synthesismentioning
confidence: 99%