Bending and Tempering Process of L415M Hot Induction Bend Used in Low Temperatures Areas

Abstract: Test bends of L415M hot induction bend of 508 mm OD×14.3 mm WT used in –45°C areas were conducted. The bending and tempering process parameters were designed, the influences of bending and tempering process parameters on impact toughness at –45°C and microstructure of tangent weld and bend weld were investigated. Hot induction bend was produced by the process of local induction heating+fast water quenching. After tempering treatment, the weld contained martensite-austenite (M-A) islands, carbide precipitations… Show more