The aim of the study was to develop a technology for welding non-weldable 42CrMo4 and NANOS-BA® steel grades in the process of hot rolling and two-stage heat treatment. As a result of physical experiments carried out in a line for semi-industrial simulation of the production of metals and their alloys (LPS) and additional heat treatment, a durable combination of 42CrMo4 and NANOS-BA® steels with high mechanical properties was obtained, including: Rp0.2 = 1036 MPa, Rm = 1504 MPa and A = 10.9%, without microscopically visible cracks and other discontinuities in the joined surface. The quality of the 42CrMo4/NANOS-BA® clad plates produced in this way was assessed on the basis of microstructure examination as well as bending, shear and tensile strength tests.