Atomic layer deposition of zinc oxide on mesoporous zirconia using zinc(II) acetylacetonate and air

Abstract: The self-terminating chemistry of atomic layer deposition (ALD) ideally enables the growth of homogeneously distributed materials on an atomic scale. This study investigates the ALD of zinc oxide (ZnO) on mesoporous zirconium oxide (ZrO2) using zinc acetylacetonate [Zn(acac)2] and synthetic air in a fixed-bed powder ALD reactor. A broad variety of methods, including thermogravimetry analysis, scanning electron microscopy with energy dispersive X-ray spectroscopy, low energy ion scattering, X-ray absorption nea… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 98 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?