Atomic layer deposition of TaN thin film on Ti–6Al–4V dental implant for enhanced anti-corrosion and anti-bacterial properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
1
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 11 publications
(5 citation statements)
references
References 42 publications
0
1
0
Order By: Relevance
“…TaN is widely used for the implant coating material due to its high mechanical strength, high chemical stability, and high biocompatibility but TaN coating also has a tremendous antibacterial effect [28]. TaN coating decreased E. coli and S. aureus colony formation due to the increased water contact angle and hydrophobic properties.…”
Section: Other Binary and More Complex Oxide Compoundsmentioning
confidence: 99%
See 3 more Smart Citations
“…TaN is widely used for the implant coating material due to its high mechanical strength, high chemical stability, and high biocompatibility but TaN coating also has a tremendous antibacterial effect [28]. TaN coating decreased E. coli and S. aureus colony formation due to the increased water contact angle and hydrophobic properties.…”
Section: Other Binary and More Complex Oxide Compoundsmentioning
confidence: 99%
“…To date, there are about ten studies that have focused on antibacterial ALD coatings for potential applications in orthopedic implants, and there have been a slightly smaller number for dental implants. Substrates tested have included flat titanium [28,49,57,96], ZrO 2 [80,87], and stainless steel [26], as well as substrates with deposited carbon nanotubes [43], titanium nanotubes [44,98], or rough SLA surfaces [26,87]. In addition, porous substrates, 3D-printed scaffolds made of titanium [27,122] and iron [86], as well as the denture material PMMA [53,63,64], have been used.…”
Section: Medical Implantsmentioning
confidence: 99%
See 2 more Smart Citations
“…Titanium alloys play an important role in the process of industrialization because of their high strength, strong corrosion resistance, and good temperature performance. The corrosion resistance of titanium alloy tubes is nearly 100 times higher than that of stainless-steel tubes, which is widely used in navigation, chemical industry, and biomedicine [1][2][3]. From the view of the overall development of the high-end industry, the high-quality mass production of titanium alloy elbow will become the core force to improve the performance of high-end equipment.…”
Section: Introductionmentioning
confidence: 99%