Antimicrobial polyurethane synthetic leather coating with In-situ generated Nano-TiO2

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
24
0
2

Year Published

2011
2011
2018
2018

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 29 publications
(26 citation statements)
references
References 11 publications
0
24
0
2
Order By: Relevance
“…The measurement of the antifungal activities of the WPU/TiO 2 films was conducted against A. niger, the most common fungus that contaminated WPU coating, illuminating on the basis of the decrease in the diameter of films [36]. As shown in Fig.…”
Section: Antifungal Capacity Testmentioning
confidence: 99%
“…The measurement of the antifungal activities of the WPU/TiO 2 films was conducted against A. niger, the most common fungus that contaminated WPU coating, illuminating on the basis of the decrease in the diameter of films [36]. As shown in Fig.…”
Section: Antifungal Capacity Testmentioning
confidence: 99%
“…Evidently, this may suggest slight antimicrobial activity of PEI/TiO 2 BNC buried in the soil. Some other experiments also showed that the antimicrobial activity of the nano-TiO 2 composites increases with increasing concentration [39] and higher antimicrobial behavior will reduce biodegradation of the polymer in the soil. It may be recommended that for synthesis of biocompatible polymers, low concentration of TiO 2 must be used.…”
Section: Soil Burial Studymentioning
confidence: 94%
“…Hal ini disebabkan adanya lapisan PU yang memberikan keunggulan fleksibilitas temperatur rendah (Chen et al, 2010). Hasil senada diperoleh oleh Shen et al (2017).…”
Section: Ketahanan Terhadap Temperatur Rendahunclassified
“…Pelapisan kulit sintetis dengan PU dapat meningkatkan ketahanan kulit sintetis terhadap cuaca dan fleksibilitas pada suhu rendah (Akovali et al, 2012;Chen et al, 2010). Coating PU dapat dilakukan dengan metode kering, basah, dan kombinasi keduanya.…”