Al2O3/chitosan nanocomposite: Preparation, characterization and kinetic study of its thermal degradation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
8
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 15 publications
(8 citation statements)
references
References 35 publications
0
8
0
Order By: Relevance
“…The VA method can also reduce the coupling errors of different parameters and yield more reliable E α . In the previous research, the apparent activation energy was obtained by model methods, such as Kissinger method, Flynn–Wall–Ozawa method, and autocatalytic method . The fitting of above three methods are simple and easy to obtain based on the actual data.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…The VA method can also reduce the coupling errors of different parameters and yield more reliable E α . In the previous research, the apparent activation energy was obtained by model methods, such as Kissinger method, Flynn–Wall–Ozawa method, and autocatalytic method . The fitting of above three methods are simple and easy to obtain based on the actual data.…”
Section: Introductionmentioning
confidence: 99%
“…2,15,16 In the previous research, the apparent activation energy was obtained by model methods, such as Kissinger method, Flynn-Wall-Ozawa method, and autocatalytic method. [17][18][19] The fitting of above three methods are simple and easy to obtain based on the actual data. In general, the local incompatibility of the curing system was existed via model methods, especially the curing process is controlled by diffusion in the late curing stage.…”
Section: Introductionmentioning
confidence: 99%
“…Figure 8 a shows the TGA curves of CS flakes and spheres. The first stage of degradation occurs between 35 °C to 200 °C, with a weight loss of approximately 12%, related to the evaporation of water molecules or small molecules [ 34 ]. According to the curve, these elements’ weight loss occurs more pronounced in the CS flakes than the CS spheres.…”
Section: Resultsmentioning
confidence: 99%
“…The second stage of degradation occurs between 200 °C to 550 °C, with a weight loss of 68% and 74%, corresponding to CS’s flakes and spheres, respectively. This stage is related to a complex process that involves the dehydration of the saccharide rings and the decomposition of the acetylated and deacetylated units of CS [ 34 ]. Furthermore, in Figure 8 b, in the DTGA curves, it can be seen that CS spheres present a first peak representing the maximum rate of degradation, which occurs at 290 °C (decomposition temperature).…”
Section: Resultsmentioning
confidence: 99%
“…There was a weight loss of 5% around 250 C. This weight loss corresponds to the desorption of physically adsorbed water on the sample surfaces. 28 Aer this temperature, the weight loss curves become increasingly pronounced up to a temperature of 450 C for samples with CS sheets and spheres, and at 470 C for the control sample. Therefore, it can be said that CS decreases the thermal stability of the bone cements.…”
Section: Morphology Studiesmentioning
confidence: 96%