1977
DOI: 10.1364/ao.16.002775
|View full text |Cite
|
Sign up to set email alerts
|

Absolute reflectance of Eastman White Reflectance Standard

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
9
0

Year Published

1979
1979
2014
2014

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 41 publications
(9 citation statements)
references
References 6 publications
(4 reference statements)
0
9
0
Order By: Relevance
“…The first commercial coating of this type was developed by Franc Grum and George William Luckey of Eastman Kodak, introduced in the 1970s [14,15]. The first commercial coating of this type was developed by Franc Grum and George William Luckey of Eastman Kodak, introduced in the 1970s [14,15].…”
Section: Sprayed-on Coatingsmentioning
confidence: 99%
“…The first commercial coating of this type was developed by Franc Grum and George William Luckey of Eastman Kodak, introduced in the 1970s [14,15]. The first commercial coating of this type was developed by Franc Grum and George William Luckey of Eastman Kodak, introduced in the 1970s [14,15].…”
Section: Sprayed-on Coatingsmentioning
confidence: 99%
“…3. The conversion was effected using the Kubelka-Munk function F(R ∞ ) [21][22][23], as given in Eq. (1), where R ∞ represents the absolute reflectance of the Dex-I␤CDP sample.…”
Section: Removal and Rebinding Of Dextromethorphanmentioning
confidence: 99%
“…For interinstrument comparisons, Eastman White Reflectance Standard20 (pressed barium sulfate) was used and was either assigned a reflectance factor of 100 at each wavelength, or assigned absolute reflectance factors from the literature. 21 Measurements were performed with the specular component either included or excluded (hereafter SIN or SEX, respectively) depending on the sample and test. Most textile measurements were made with the specular component included (SIN mode).…”
Section: Instrumentsmentioning
confidence: 99%