2017
DOI: 10.1016/j.actamat.2017.03.069
|View full text |Cite
|
Sign up to set email alerts
|

A TRIP-assisted dual-phase high-entropy alloy: Grain size and phase fraction effects on deformation behavior

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

4
171
0

Year Published

2017
2017
2020
2020

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 508 publications
(175 citation statements)
references
References 66 publications
4
171
0
Order By: Relevance
“…Long-term annealing treatments (e.g., 500 days) at intermediate temperatures (e.g., 700°C and 500°C) can lead to chemical segregations even for the single-phase equiatomic CoCrFeMnNi HEA. 8 Interestingly, for the recently designed TRIPassisted dual-phase HEAs, 13 annealing treatments can be used not only to control the grain size, but also to modify the phase fractions in the microstructure. Figure 4 shows the variations in the FCC grain size and HCP phase fraction of the quaternary dual-phase Fe 50 Mn 30 Co 10 Cr 10 HEA with increasing annealing time at 900°C.…”
Section: Processing Of Strong and Ductile Bulk Non-equiatomic High-enmentioning
confidence: 99%
See 4 more Smart Citations
“…Long-term annealing treatments (e.g., 500 days) at intermediate temperatures (e.g., 700°C and 500°C) can lead to chemical segregations even for the single-phase equiatomic CoCrFeMnNi HEA. 8 Interestingly, for the recently designed TRIPassisted dual-phase HEAs, 13 annealing treatments can be used not only to control the grain size, but also to modify the phase fractions in the microstructure. Figure 4 shows the variations in the FCC grain size and HCP phase fraction of the quaternary dual-phase Fe 50 Mn 30 Co 10 Cr 10 HEA with increasing annealing time at 900°C.…”
Section: Processing Of Strong and Ductile Bulk Non-equiatomic High-enmentioning
confidence: 99%
“…Figure 4 shows the variations in the FCC grain size and HCP phase fraction of the quaternary dual-phase Fe 50 Mn 30 Co 10 Cr 10 HEA with increasing annealing time at 900°C. 13 In cold-rolled condition, the alloy shows average grain size of $250 nm and HCP phase fraction of $91%. After extending the annealing time from 3 min to 60 min, the average FCC grain size increased gradually from $4.5 lm to $17.5 lm.…”
Section: Processing Of Strong and Ductile Bulk Non-equiatomic High-enmentioning
confidence: 99%