“…29 Further, graphite was oxidized via a modified Hummer method, and due to this, graphite converts into GO, which shows a new peak in Figure 2(b) at 2 θ = 11.42°. 2 In addition, the XRD spectra were also used for calculating the number of layers of GO, and we have found that two to three layers 30 –33 are in good agreement with the Raman spectra of GO. After this process, GO was reduced via hydrazine hydrate, which converts the GO into the rGO, with the characteristics broad peak of rGO to be 2 θ = 28.71° (Figure 2(c)).…”