2020
DOI: 10.1016/j.mattod.2019.07.002
|View full text |Cite
|
Sign up to set email alerts
|

A reality check and tutorial on electrochemical characterization of battery cell materials: How to choose the appropriate cell setup

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

2
231
0

Year Published

2020
2020
2022
2022

Publication Types

Select...
7
1

Relationship

5
3

Authors

Journals

citations
Cited by 201 publications
(234 citation statements)
references
References 136 publications
2
231
0
Order By: Relevance
“…impact of the use of Li metal as anode. From experience of lab and commercial cell behavior, irreproducible, high and abnormal deviations in the specific charge capacities during cycling, particularly during C-rate tests, may be attributed to the Li metal negative electrode (in three electrode arrangement: Li as counter electrode) 36 . An indication is e.g.…”
Section: Results and Discussion Failure During Charge: Impact Of Peo mentioning
confidence: 99%
See 1 more Smart Citation
“…impact of the use of Li metal as anode. From experience of lab and commercial cell behavior, irreproducible, high and abnormal deviations in the specific charge capacities during cycling, particularly during C-rate tests, may be attributed to the Li metal negative electrode (in three electrode arrangement: Li as counter electrode) 36 . An indication is e.g.…”
Section: Results and Discussion Failure During Charge: Impact Of Peo mentioning
confidence: 99%
“…All cells used in galvanostatic cycling tests were prepared in two electrode setup (coin cell) using the above mentioned positive electrodes as working electrode, PEO-LiTFSI as polymer membrane and lithium metal or graphite as negative electrode. Cells used for the determination of the oxidative stability were prepared in three-electrode setup using the above mentioned positive electrodes as working electrode, and lithium metal as counter and reference electrode 36 . Stated membrane thicknesses refer to the thickness before cell assembly at room temperature.…”
Section: Electrode Preparation and Cell Assembly Nmc 622 Electrodes mentioning
confidence: 99%
“…The SSLSBs were assembled by stacking the lithium metal anode, LCE, and S/PAN cathode in 2032‐coin cell setup in an argon‐filled glovebox 64. The galvanostatic cycling was performed on a MACCOR Series 4000 battery tester at 60 °C.…”
Section: Methodsmentioning
confidence: 99%
“…The electrochemical characterization of the Li p ‐electrodes was carried out in 2‐electrode [ 32 ] coin cells (CR2032) using a battery tester Maccor Series 4000 (Maccor Inc.). For this, Cu||Li p and NMC||Li p cells with a separator stack including four layers of non‐woven poly(propylene) separators (Freudenberg, FS 2190) faced to the Cu‐foil and one layer of Celgard 2500 separator facing to the Li side were used.…”
mentioning