2017
DOI: 10.1016/j.cej.2017.06.144
|View full text |Cite
|
Sign up to set email alerts
|

A novel hierarchical hollow SiO 2 @MnO 2 cubes reinforced elastic polyurethane foam for the highly efficient removal of oil from water

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
30
0

Year Published

2019
2019
2023
2023

Publication Types

Select...
10

Relationship

0
10

Authors

Journals

citations
Cited by 92 publications
(32 citation statements)
references
References 22 publications
0
30
0
Order By: Relevance
“…To prepare SiO 2 @Mn x O y , the silica spheres (0.3 g) were dispersed in DI water (20 mL) at 30 C for 1 h using ultrasonication, 27 followed by the addition of KMnO 4 (0.015-1.8 g) or Mn(CH 3 CO) 2 $4H 2 O (or Mn-acetate, 0.15-1.8 g). Subsequently, the suspension was transferred to a Teon-lined stainless-steel autoclave-type reactor and heated to 150 C at a heating rate of 10 C min À1 ; the temperature was maintained at 150 C for 48 h. [28][29][30] The autoclave-type reactor was then cooled to room temperature under ambient conditions. Subsequently, the SiO 2 @MnO x (KMnO 4 ) and SiO 2 @-MnO x (Mn-acetate) core-shell structures were collected by centrifugation and washed ve times or more with ethanol and DI water.…”
Section: Preparation Of Sio 2 @Mno Xmentioning
confidence: 99%
“…To prepare SiO 2 @Mn x O y , the silica spheres (0.3 g) were dispersed in DI water (20 mL) at 30 C for 1 h using ultrasonication, 27 followed by the addition of KMnO 4 (0.015-1.8 g) or Mn(CH 3 CO) 2 $4H 2 O (or Mn-acetate, 0.15-1.8 g). Subsequently, the suspension was transferred to a Teon-lined stainless-steel autoclave-type reactor and heated to 150 C at a heating rate of 10 C min À1 ; the temperature was maintained at 150 C for 48 h. [28][29][30] The autoclave-type reactor was then cooled to room temperature under ambient conditions. Subsequently, the SiO 2 @MnO x (KMnO 4 ) and SiO 2 @-MnO x (Mn-acetate) core-shell structures were collected by centrifugation and washed ve times or more with ethanol and DI water.…”
Section: Preparation Of Sio 2 @Mno Xmentioning
confidence: 99%
“…Cao et al investigated the PU sponge fictionalized with super‐hydrophobic nano‐diamond particles. Yuan et al thoughts that SiO 2 @MnO 2 cubes reinforced PU foam for the highly efficient removal of oil from water and the composite PU foam showed excellent elasticity. Kong et al studied the fabrication of hydrophobic Al 2 O 3 /PU foam for oil/water separation and it deduced that the absorption capacity of Al 2 O 3 /PU had good potential application in oil‐water separation.…”
Section: Introductionmentioning
confidence: 99%
“…Pan et al [23] and coworkers prepared hydrophobic polyvinyl formaldehyde sponges by one-step surface modification, but massive pyridine, a strong virose organic reagent, is involved as the solvent. Yuan [24] and coworkers designed a hollow SiO 2 @MnO 2 modified PU foam for high-efficiency oil-water separation; however, MnO 2 may introduce heavy metals (Mn 4+ ) and lead to secondary pollution. Given limits of the cases discussed above, we raised a facile and green one-pot synthesis of silylated PVA sponge for oil-water separation, possessing advantages (e.g., high porosity, stable structure, and low cost).…”