A modulated differential scanning calorimetry and small-angle x-ray scattering study of the interfacial region in structured latices

Abstract: A interface de latexes de poliestireno (PS)-poliacrilato de metila (PMA) foi investigada por calorimetria diferencial de varredura no modo modulado (DSC-modulado) e por espalhamento de raios-x de baixo ângulo (SAXS). A fração em massa da interface destes latexes foi estimada através do sinal do DSC-modulado, dCp/dt. Foi encontrado o valor de 13% para latexes de PS-PMA (1:1 em massa) contendo PS reticulado com diferentes densidades de reticulação (0, 1, 3, 5 e 10 mol% de agente reticulante). O aumento da densid… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
8
0

Year Published

2005
2005
2017
2017

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 11 publications
(8 citation statements)
references
References 15 publications
0
8
0
Order By: Relevance
“…Modulated DSC has been shown to be very useful to quantify the amount of polymer present within interfacial regions in polymer blends15–17 as well as to monitor the extent of phase separation during polymerization reactions 18. In fact, Karlsson et al used both DSC and dynamic mechanical analysis (DMA) to study the amount of interphase and the mechanical properties of films derived from both composite latices and from latex blends 19.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Modulated DSC has been shown to be very useful to quantify the amount of polymer present within interfacial regions in polymer blends15–17 as well as to monitor the extent of phase separation during polymerization reactions 18. In fact, Karlsson et al used both DSC and dynamic mechanical analysis (DMA) to study the amount of interphase and the mechanical properties of films derived from both composite latices and from latex blends 19.…”
Section: Introductionmentioning
confidence: 99%
“…In fact, Karlsson et al used both DSC and dynamic mechanical analysis (DMA) to study the amount of interphase and the mechanical properties of films derived from both composite latices and from latex blends 19. One straightforward approach15–17 is to compare the value of the Δ C p at the glass transitions to the values expected for the corresponding pure polymers. It is often found that the Δ C p in a composite is less than expected, and the difference is attributed to polymer that is present within the polymer/polymer interfacial zones.…”
Section: Introductionmentioning
confidence: 99%
“…MDSC was used to investigate the effect of the cross-link density of a polystyrene seed on the thickness of the interfacial region in the polystyrene/poly(methyl acrylate) (PS/PMA) particles synthesized by seeded polymerization [84]. The weight fraction of interfacial region was evaluated on the basis of depletion of dCp/dT for PS/PMA compared to dCp/dT values for pure components.…”
Section: Non-microscopical Quantitative Methods Of Core-shell Morphomentioning
confidence: 99%
“…The second system used a seed polymer of poly(butyl acrylate‐ co ‐St) [P(BA‐ co ‐St)] with MMA as the second‐stage monomer, representing a CS system. The MWDs of the resulting second‐stage polymers were determined using gel permeation chromatography (GPC) and the morphologies of the composite particles were characterized using transmission electron microscopy (TEM), differential scanning calorimetry (DSC),15, 30–33 and surfactant titration 34–37…”
Section: Methodsmentioning
confidence: 99%