2019
DOI: 10.1016/j.actbio.2019.08.034
|View full text |Cite
|
Sign up to set email alerts
|

A manufacturing and annealing protocol to develop a cold-sprayed Fe-316L stainless steel biodegradable stenting material

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 15 publications
(4 citation statements)
references
References 56 publications
0
4
0
Order By: Relevance
“…All the Zn coatings show higher FWHM than the Zn powder, and Zn coatings after heat treatment show lower FWHM than the as-sprayed Zn coating. FWHM is typically relative to the grain refinement, residual stress, and plastic deformation within the cold-sprayed metal coatings [ 16 , 26 ]. Peak broadening, as well as the increase in FWHM, can be attributed to an accumulation of stacking faults and structural disorders, grain refinement as well as increased stress [ 12 ].…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…All the Zn coatings show higher FWHM than the Zn powder, and Zn coatings after heat treatment show lower FWHM than the as-sprayed Zn coating. FWHM is typically relative to the grain refinement, residual stress, and plastic deformation within the cold-sprayed metal coatings [ 16 , 26 ]. Peak broadening, as well as the increase in FWHM, can be attributed to an accumulation of stacking faults and structural disorders, grain refinement as well as increased stress [ 12 ].…”
Section: Resultsmentioning
confidence: 99%
“…Cold-sprayed metal coatings are formed by plastic deformations of metal particles due to the high-velocity impact. The inter-particle bonding interface and the coating/substrate interface are weak and mechanically interlocked, which results in overall poor ductility with brittle fractures commonly occurring [ 16 , 17 ]. To attain higher bonding strength and promote the overall coating performance, post-process heat treatment is usually conducted on the cold-sprayed coating.…”
Section: Introductionmentioning
confidence: 99%
“… −0.824 vs. SCE 73.4 0.85 N.A. [ 58 ] Annealed Fe at 1100 °C 274 104 N.A. Between −0.55 and −0.6 V vs. SCE N.A.…”
Section: Strategy To Accelerate Fe Corrosionmentioning
confidence: 99%
“…An in-depth review of the advancements in manufacturing and processing can be found in this recent article [ 56 ]. One of the additively manufacturing techniques, to obtain Fe surface with desired defects and grain refinement for degradation, is called cold gas dynamic spraying [ 58 ]. It is a high-pressure powder processing technique, utilizing compressed gas to propel metal powder at a large temperature range.…”
Section: Strategy To Accelerate Fe Corrosionmentioning
confidence: 99%