A conductometric enzymatic methanol sensor based on polystyrene - PAMAM dendritic polymer electrospun nanofibers

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2023
2023
2023
2023

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(2 citation statements)
references
References 29 publications
0
2
0
Order By: Relevance
“…Razmshoar et al [ 35 ] created a conductometric enzymatic methanol sensor by grafting alcohol oxidase (AOx) onto electrospun polystyrene-poly(amidoamine) dendritic polymer nanofibers. To form a strong link between AOx and the surface of nanofibers, glutaraldehyde coupling was used to form a bond between the amine groups of the AOx enzyme and the nanofiber dendritic polymer groups ( Figure 6 a).…”
Section: The Immobilization Methods Of Enzymementioning
confidence: 99%
See 1 more Smart Citation
“…Razmshoar et al [ 35 ] created a conductometric enzymatic methanol sensor by grafting alcohol oxidase (AOx) onto electrospun polystyrene-poly(amidoamine) dendritic polymer nanofibers. To form a strong link between AOx and the surface of nanofibers, glutaraldehyde coupling was used to form a bond between the amine groups of the AOx enzyme and the nanofiber dendritic polymer groups ( Figure 6 a).…”
Section: The Immobilization Methods Of Enzymementioning
confidence: 99%
“… ( a ) The schematic of preparation alcohol oxidase-based methanol sensor; ( b ) FTIR spectra of PS-PAMAM, GA-PS-PAMAM, and AOX/PS-PAMAM ESNFs samples; ( c ) the response of sensor to a series concentration of gas-phase methanol [ 35 ]; ( d ) The schematic diagram of the process for preparing paper-based ethanol biosensor; ( e ) The calibration plot of ethanol concentration vs. current (The inset shows the chronoamperometric records with the concentration increase from 0–12 mM); ( f ) the evaluation of shelf-life at 4 °C of the ethanol sensor, fresh biosensor (black bar), 1 week (red bar), 2 weeks (green bar), 3 weeks (blue bar) and 4 weeks (violet bar) [ 19 ]. …”
Section: Figurementioning
confidence: 99%