A conductive PVDF-Ni membrane with superior rejection, permeance and antifouling ability via electric assisted in-situ aeration for dye separation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
37
0
3

Year Published

2019
2019
2023
2023

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 110 publications
(40 citation statements)
references
References 69 publications
0
37
0
3
Order By: Relevance
“…2(b), the O 1s spectrum was tted, consisting mainly of two components, one is 529.7 eV (Mn-O-Mn) and the other is 531.6 eV (Mn-OH), which is in good agreement with the ref. [38][39][40]. Hence, aer comprehensive analysis, we could conclude that the deposited lm is MnO 2 $nH 2 O.…”
Section: Tem and Xps Analysismentioning
confidence: 82%
“…2(b), the O 1s spectrum was tted, consisting mainly of two components, one is 529.7 eV (Mn-O-Mn) and the other is 531.6 eV (Mn-OH), which is in good agreement with the ref. [38][39][40]. Hence, aer comprehensive analysis, we could conclude that the deposited lm is MnO 2 $nH 2 O.…”
Section: Tem and Xps Analysismentioning
confidence: 82%
“…To obtain a hydrodynamic understanding of the membrane fouling, an interpretation of the membrane fouling mechanism can be now developed from the extended Derjaguin-Landau-Verwey-Overbeek (XDLVO) theory (Lee et al, 2007;Hong et al, 2013;Lin T. et al, 2014). Based on the XDLVO theory, the fouling process can be quantitatively evaluated via the interface thermodynamic reactions (Shen et al, 2015(Shen et al, , 2017bYu et al, 2019). Theoretically, a membrane that presents lower roughness, an enhanced negative charge, and a hydrophilic surface will show less adhesion force toward NOM present in wastewater (Zhang et al, 2015).…”
Section: Membrane Foulingmentioning
confidence: 99%
“…The external modification refers to physically or chemically coating hydrophilic components onto the membrane surface (Yu et al, 2019;Zhao et al, 2019). During the membrane fouling process, pollutants firstly get closer to the membrane surface, then interact with the membrane surface, and eventually adhere to the membrane surface.…”
Section: Modification Technologymentioning
confidence: 99%
“…The whole composite was exposed in the air for 10.0 s followed by immersing into a DI water bath to initiate phase inversion process. Once the substrate was peeled off from the glass plate, it was removed from the water bath, thoroughly rinsed with DI water for three times and then transferred to a 4 • C DI water bath for storage till later use (Qin et al, 2013;Shen et al, 2015;Yu et al, 2019).…”
Section: The Preparation Of Polysufone (Psf) Substratementioning