2002
DOI: 10.1023/a:1020893609476
|View full text |Cite
|
Sign up to set email alerts
|

Untitled

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
0
0

Year Published

2003
2003
2013
2013

Publication Types

Select...
3

Relationship

0
3

Authors

Journals

citations
Cited by 3 publications
(1 citation statement)
references
References 10 publications
0
0
0
Order By: Relevance
“…Table 5 shows that with increasing amount of superfine mineral powder, the initial slump and slump flow increase. The reason is that the superfine mineral powder has microfilling and dispersion properties [8] .The 3d strength of concrete reduces and 28d strength increases significantly, which result from the secondary hydration of superfine mineral powder. The above results show that ZJ04 has better performances in various aspects.…”
Section: Concrete Mixing Proportionsmentioning
confidence: 99%
“…Table 5 shows that with increasing amount of superfine mineral powder, the initial slump and slump flow increase. The reason is that the superfine mineral powder has microfilling and dispersion properties [8] .The 3d strength of concrete reduces and 28d strength increases significantly, which result from the secondary hydration of superfine mineral powder. The above results show that ZJ04 has better performances in various aspects.…”
Section: Concrete Mixing Proportionsmentioning
confidence: 99%