Preparation and Characterization of Nanowhiskers Cellulose from Fiber Arrowroot (Maranta arundinacea)

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
6
0

Year Published

2017
2017
2022
2022

Publication Types

Select...
9
1

Relationship

0
10

Authors

Journals

citations
Cited by 21 publications
(6 citation statements)
references
References 14 publications
0
6
0
Order By: Relevance
“…The C-O vibration stretching resulted from the uronic and acetyl ester groups; from hemicellulose, pectin or the ester of carboxylic group of p-coumaric and ferulic acids of hemicellulose or lignin. C-O-C pyranose ring was attributed to the structure of cellulose its stretching vibration is at 1058.9 cm −1 [20]. In cellulosic samples, the spectral ratio of 1431.18 cm −1 provides the evidence of containing cellulose (Fig.…”
Section: Ftir Analysismentioning
confidence: 96%
“…The C-O vibration stretching resulted from the uronic and acetyl ester groups; from hemicellulose, pectin or the ester of carboxylic group of p-coumaric and ferulic acids of hemicellulose or lignin. C-O-C pyranose ring was attributed to the structure of cellulose its stretching vibration is at 1058.9 cm −1 [20]. In cellulosic samples, the spectral ratio of 1431.18 cm −1 provides the evidence of containing cellulose (Fig.…”
Section: Ftir Analysismentioning
confidence: 96%
“…The production of cellulose nanocrystals from different lignocellulosic fibers has attracted interest in the scientific and industrial community in recent years. This has been owing to their mechanical and thermal properties, cost effectiveness, and versatility [20,21] . Nanocrystals are generally characterized by high solidity and crystallinity, which afford sustainability.…”
Section: Introductionmentioning
confidence: 99%
“…This procedure ensures the removal of all residual NaOH in the fiber. The samples were then dried in an oven at 100°C until reaching a constant mass (Sá, Miranda & José, 2015;Miranda, Fiuza, Carvalho & José, 2015).…”