The 7A09 aluminum alloy was subjected to T6 heat treatment by means of microstructure analysis and mechanical property testing. The results show that the best solid solution treatment process of 7A09 aluminum alloy is 470°C*1 hr. The transverse tensile strength of 7A09 aluminum alloy reaches 555.9MPa, the elongation of 7A09 aluminum alloy reaches 13.5%, and the cloth hardness reaches 152.6HBW. Compared with the cast aluminum alloy, the tensile strength, elongation and hardness increase by 10.3%, 8% and 13.5% respectively, and the mechanical properties of 7A09 aluminum alloy are significantly improved. The mechanical properties of the alloy are significantly improved.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.