In this study, Eucalyptus globulus stumpwood samples collected from six different sites in Portugal were evaluated for their ease of pulping, using two delignification processes (kraft and alkaline sulfite-anthraquinonemethanol (ASAM)). Morphologically, the stumpwood included fibers with a mean length of 0.930 mm, diameter of 21.4 µm, lumen width of 9.1 µm, and cell-wall thickness of 6.1 µm. The Runkel ratio varied between 1.0 and 1.9, and the slenderness ratio ranged between 50.6 and 35.1. ASAM pulps presented higher yields and kappa numbers (49.3% and 36, respectively) when compared to kraft pulps (42.7% and 14, respectively). Extractive-free material increased pulp yield (51.7% and 47.5% for ASAM and kraft, respectively) and decreased kappa number (18 and 11). The kraft pulps showed a coarseness of 0.096 mg/m, curl of 5.2%, and 16.7% kinked fibers, while for the ASAM pulps, these values were 0.105 mg/m, 5.2%, and 16.3%, respectively.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.