Abstract: The wear behaviour on prealloyed sintered steel parts TiCN PVD coating was analysed. Cylindrical specimens ( 40x30 mm3) were compacted to the green density of ~7.0 g.cm-3. The specimens were sintered in pusher furnace at the temperature of 1180°C for 40 minutes in an atmosphere of 25H2+75N2. Part of sintered specimens was then coated by Physical Vapour Deposition. Wear tests were carried out by means of a pin-on-disk tribometer. The results of profilograms (the values of surface roughness) and the wear curves…