Untersuchungen zur Optimierung von Holzfaserdämmstoffen in Abhängigkeit von Rohstoff, Herstellverfahren und Aufschlussbedingungen

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2020
2020
2020
2020

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…The thermal conductivity of the comparable GUTEX product (180 kg/m³, 40 mm) is 0.043 W/mK (GUTEX 2019a). After loosening, gluing and re-compacting to 180 kg/m³ and a thickness of 40 mm, a thermal conductivity between 0.043 and 0.044 W/mK was measurable, indicating that thermal conductivity is in particular dependent on the density and moisture content of the board and not on type of binding agent or board thickness (Foglia 2006;Sonderegger and Niemz 2009;Brombacher 2015).…”
Section: Physical-technological Properties Of Wfimentioning
confidence: 99%
“…The thermal conductivity of the comparable GUTEX product (180 kg/m³, 40 mm) is 0.043 W/mK (GUTEX 2019a). After loosening, gluing and re-compacting to 180 kg/m³ and a thickness of 40 mm, a thermal conductivity between 0.043 and 0.044 W/mK was measurable, indicating that thermal conductivity is in particular dependent on the density and moisture content of the board and not on type of binding agent or board thickness (Foglia 2006;Sonderegger and Niemz 2009;Brombacher 2015).…”
Section: Physical-technological Properties Of Wfimentioning
confidence: 99%