2014
DOI: 10.1007/s40544-014-0043-5
|View full text |Cite
|
Sign up to set email alerts
|

Tribological properties of short carbon fibers reinforced epoxy composites

Abstract: Short carbon fiber (SCF) reinforced epoxy composites with different SCF contents were developed to investigate their tribological properties. The friction coefficient and wear of the epoxy composites slid in a circular path against a steel pin inclined at 45° to a vertical axis and a steel ball significantly decreased with increased SCF content due to the solid lubricating effect of SCFs along with the improved mechanical strength of the composites. The scanning electron microscope (SEM) observation showed tha… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

2
40
0

Year Published

2014
2014
2024
2024

Publication Types

Select...
6
1

Relationship

2
5

Authors

Journals

citations
Cited by 66 publications
(46 citation statements)
references
References 53 publications
2
40
0
Order By: Relevance
“…The mixture was evacuated for about 15 min to completely remove air-bubbles and then molded in Teflon molds for pure epoxy samples. For the epoxy composite samples with 8 wt.% SCFs, the degassed epoxy resin was mixed with SCFs at different concentrations in a glass beaker placed in a water bath at 60 C and mechanically stirred at 1500 rpm for 30 min [19]. After degassing for 15 min in a vacuum oven, the hardener was added in the mixture followed by hand stirring for 10 min and degassing for another 15 min.…”
Section: Samplementioning
confidence: 99%
See 3 more Smart Citations
“…The mixture was evacuated for about 15 min to completely remove air-bubbles and then molded in Teflon molds for pure epoxy samples. For the epoxy composite samples with 8 wt.% SCFs, the degassed epoxy resin was mixed with SCFs at different concentrations in a glass beaker placed in a water bath at 60 C and mechanically stirred at 1500 rpm for 30 min [19]. After degassing for 15 min in a vacuum oven, the hardener was added in the mixture followed by hand stirring for 10 min and degassing for another 15 min.…”
Section: Samplementioning
confidence: 99%
“…Therefore, it is importantly necessary to improve the mechanical strength of polymer composites while maintaining their relatively low friction and wear for oil and gas applications (e.g., flexible risers) where high mechanical strength, low friction, and excellent wear resistance are crucial. SCFs can be considered as one of the most popular candidates for the development of high strength polymer composites because of their high surfaceto-volume ratio, outstanding thermal and mechanical properties, and good dispersion in polymer matrices [17][18][19]. Moreover, SCFs can serve as a solid lubricant to lubricate rubbing surfaces for friction reducing applications [19][20][21][22][23][24].…”
Section: Introductionmentioning
confidence: 99%
See 2 more Smart Citations
“…Liquid epoxy resins exhibit better mixing and processing abilities with reinforcement materials in granular or fiber form and the mixtures result in composite materials with intermediate properties depending on combined actions of 19.1 Introduction the components [12]. In addition, epoxy resins represent an important class of polymers due to their excellent adhesion to many substrates, high tensile, compressive and flexural strength, and high chemical, fatigue, and corrosion electrical resistance [13][14][15].…”
Section: Introductionmentioning
confidence: 99%