2013
DOI: 10.1177/0021998313511652
|View full text |Cite
|
Sign up to set email alerts
|

The influence of hot pressing conditions on mechanical properties of nickel aluminide/alumina composite

Abstract: The influence of hot pressing conditions on mechanical properties of nickel aluminide/alumina composite has been investigated in the present paper. In particular, effect of the process parameters, viz. compacting pressure, sintering temperature and sintering time on the evolution of density, elastic constants and tensile strength properties of the intermetallic-ceramic composite has been studied. Elastic constants, the Young's modulus and Poisson's ratio, have been evaluated using an ultrasonic testing method,… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
14
0

Year Published

2014
2014
2023
2023

Publication Types

Select...
9

Relationship

4
5

Authors

Journals

citations
Cited by 22 publications
(16 citation statements)
references
References 29 publications
2
14
0
Order By: Relevance
“…An investigation has been done to determine mechanical properties such as elastic and tensile strength of NiAl/Al 2 O 3 composite by influence of compacting pressure, sintering temperature and time. From the study, NiAl/Al 2 O 3 composite shows the highest tensile strength of 227 MPa at 0.99 relative densities which is closely in agreement that the strength of sintered material increases with increasing density [17]. Furthermore, NiAl/Al 2 O 3 composite with 1 µm NiAl particles at 15% weight fraction showed the best fracture toughness of ~8.1 MPa.m 1/2 about 80% improvement and exhibits crackhealing properties over pure alumina.…”
Section: Effect Of Ceramics In Bond Coat Propertiessupporting
confidence: 75%
“…An investigation has been done to determine mechanical properties such as elastic and tensile strength of NiAl/Al 2 O 3 composite by influence of compacting pressure, sintering temperature and time. From the study, NiAl/Al 2 O 3 composite shows the highest tensile strength of 227 MPa at 0.99 relative densities which is closely in agreement that the strength of sintered material increases with increasing density [17]. Furthermore, NiAl/Al 2 O 3 composite with 1 µm NiAl particles at 15% weight fraction showed the best fracture toughness of ~8.1 MPa.m 1/2 about 80% improvement and exhibits crackhealing properties over pure alumina.…”
Section: Effect Of Ceramics In Bond Coat Propertiessupporting
confidence: 75%
“…• C), high value of Young's modulus (stable when increasing temperature), high mechanical, fatigue, tensile and compressive strengths (also at high temperatures), and good frictional wear resistance [30][31][32].…”
Section: Metal-ceramic Functionally Graded Materials -Manufacturing mentioning
confidence: 99%
“…The same powder material has been used in experimental investigation of the complete hot pressing process presented in [2,17]. Those studies were focused on the densification during the sintering stage.…”
Section: Experimental Studiesmentioning
confidence: 99%