Synthesis of zinc oxide nanoparticles by homogeneous precipitation method and its application in antifungal activity against Candida albicans

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

3
36
0

Year Published

2015
2015
2023
2023

Publication Types

Select...
8
1

Relationship

1
8

Authors

Journals

citations
Cited by 138 publications
(51 citation statements)
references
References 41 publications
3
36
0
Order By: Relevance
“…The band at 1653 cm -1 present in the spectrum of the as-prepared sample is assigned to bending vibrations of water molecules [45]. In the spectrum of the as-prepared sample the band at 1322 cm -1 is attributed to the symmetric C=O bond vibrations [44].The band at about 833 cm -1 in the asprepared sample is due to Fe-OH bond vibrations [33]. The peak appearing in the region of 669 cm -1 is due to the presence of hydroxyl group in the as-prepared sample [46].…”
Section: Resultsmentioning
confidence: 98%
See 1 more Smart Citation
“…The band at 1653 cm -1 present in the spectrum of the as-prepared sample is assigned to bending vibrations of water molecules [45]. In the spectrum of the as-prepared sample the band at 1322 cm -1 is attributed to the symmetric C=O bond vibrations [44].The band at about 833 cm -1 in the asprepared sample is due to Fe-OH bond vibrations [33]. The peak appearing in the region of 669 cm -1 is due to the presence of hydroxyl group in the as-prepared sample [46].…”
Section: Resultsmentioning
confidence: 98%
“…3. The broad band observed in the region 3363 cm −1 corresponds to O-H stretching vibrations arising from the moisture present in KBr which is used for making pellets in an open air [44]. The band at 1653 cm -1 present in the spectrum of the as-prepared sample is assigned to bending vibrations of water molecules [45].…”
Section: Resultsmentioning
confidence: 98%
“…Figure 1 shows that particles were <100 nm with uneven size and shape (circular, oval, stretched or even irregular shape). This may be the result of the synthesis protocol used to manufacture these nanoparticles since morphological uniformity of nZnO may be obtained by optimising the calcination temperature45 or by adjusting the concentration of the ionic template such as potassium nitrate, potassium sulphate or lithium nitrate at different molar ratios46 or many other parameters depending on the synthesis protocol used. Particles were found to have a diameter ranging from 6 nm to 60 nm.…”
Section: Resultsmentioning
confidence: 99%
“…In recent past, microbial infections have become a global health burden due to emerging and resistant strains of viruses [ 1 ], bacteria [ 2 ], pathogenic fungi [ 3 ] and protozoa [ 4 ] defying clinical treatment. Consequently, this has culminated into prolonged treatment, higher health expenditure, mortality risk, and low life expectancy [ 2 ].…”
Section: Introductionmentioning
confidence: 99%