DOI: 10.3390/polym14112162
|View full text |Cite
|
Sign up to set email alerts
|

Abstract: The interface of multi-layer insulation is a relatively weak point in the cable system during the long-term high-temperature service. Space charge is prone to continuously accumulate in the interface area, leading to the deterioration of electrical properties and even insulation failure in advance. The knowledge about thermal oxidation of polyethylene (PE) materials at the molecular level is still urgent to explore. Herein, single-layer and double-layer PE insulation, representing the typical insulation struct… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2022
2022
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 25 publications
0
1
0
Order By: Relevance
“…Both studies and experience demonstrate that the interface is a weakness of composite insulation equipment [9,10]. Interfaces are often damaged by ageing and superficial erosion and cause cascading failures during long-term operations.…”
Section: Introductionmentioning
confidence: 99%
“…Both studies and experience demonstrate that the interface is a weakness of composite insulation equipment [9,10]. Interfaces are often damaged by ageing and superficial erosion and cause cascading failures during long-term operations.…”
Section: Introductionmentioning
confidence: 99%