Abstract: Abstract Terpolymerization was investigated by dilatometry for zincacrylate (ZnA2), acrylonitrile (AN), and styrene (St), radically initiated by a As2S3‐styrene complex (I) in dimethyl sulphoxide (DMSO), at 90 ± 0.1°C for 1 h under inert atmosphere. The system follows non‐ideal kinetics, due to primary radical termination as well as a degradative chain transfer reaction. The kinetic expression for the system is Rpα(I)0.27 (St)0.31 (AN) 0.22[ZnA2]0.12. The value for the activation energy and k italicp2/kt are …