2021
DOI: 10.17350/hjse19030000241
|View full text |Cite
|
Sign up to set email alerts
|

Production and Characterization of Palm Oil Based Epoxy Biocomposite by RSM Design

Abstract: T oday, social awareness of the environmental impacts of plastics is increasing, and therefore environmentally friendly materials are sought for the plastics industry [1][2][3][4]. For this reason, in addition to being environmentally friendly, the tendency towards natural fibers is increasing due to their low cost, easy processing, low density, good corrosion resistance, and high strength in wide industrial applications [5][6][7][8][9][10][11][12][13][14]. Moreover, natural fibers become an alternative to gla… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
9
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
8

Relationship

2
6

Authors

Journals

citations
Cited by 19 publications
(12 citation statements)
references
References 63 publications
(67 reference statements)
0
9
0
Order By: Relevance
“…Model equations for density, Shore D hardness, thermal conductivity coefficient, and activation energies are found to be consistent with the experimental results. Low‐error functions, high‐ R 2 values, and low‐significance values ( p‐value ) have increased the reliability of RSM results 44 …”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…Model equations for density, Shore D hardness, thermal conductivity coefficient, and activation energies are found to be consistent with the experimental results. Low‐error functions, high‐ R 2 values, and low‐significance values ( p‐value ) have increased the reliability of RSM results 44 …”
Section: Resultsmentioning
confidence: 99%
“…are added to cause a chemical reaction. The product, which has been synthesized by mixing at high speed (1500 rpm) and 120 s, is poured into standard molds and waited for curing time (Ct) for 24 h 49,50 . The experimental design of the biocomposite synthesized according to RSM design is given in Table 1.…”
Section: Methodsmentioning
confidence: 99%
“…After the curing process (24 hours) of the obtained epoxy composite is done, the necessary physical and chemical tests are carried out. The properties of the composite are determined by FTIR, SEM, density, Shore D hardness, thermal conductivity coefficient, and thermal stability tests [39][40][41]. Table 1 shows the amounts of components used in the epoxy composite production process.…”
Section: Methodsmentioning
confidence: 99%
“…According to the results obtained in this study, optimum composite production was made with 5 wt.% biomass reinforcement. Higher filler reinforcement negatively affected both the mechanical properties and surface morphology of the composite [43][44][45][46][47][48][49][50][51]. SEM images of pure and biomass reinforced composites are given in Figure 6 and Figure 7.…”
Section: Conclusion and Recommendationsmentioning
confidence: 99%